Lithium Corrosion
April 1, 2024•Material Attacked by Lithium Corrosion Experiment (MALiCE).
•Extended static molten lithium exposure.
•6 individual canisters.
•Canisters held at 1 to 5 PSI of Ar during exposure.
•Spinning Lithium Attacked Potential Substrates (SLAPS).
•Extended dynamic molten lithium exposure.
•8 samples in 1 experimental session.
•Corrosion tests conducted under high vacuum.